Brazing Flux in Saudi Arabia: Products, Specifications, and Verified Suppliers
Brazing flux is a chemical compound applied to metal joints before and during heating to prevent oxidation, clean the surface, and allow filler metal to flow and bond correctly. Without flux, oxygen reacts with heated metal and forms oxides that block the filler from wetting the base material. This page covers the types of brazing flux available in Saudi Arabia, the products stocked by regional distributors, and direct supplier contacts for procurement in Riyadh, Jeddah, Dammam, and the Eastern Province.
Quick Reference
Most industrial buyers in Saudi Arabia source white brazing flux for silver and copper work, borax-based flux for steel and brass, and aluminium brazing flux for refrigeration and HVAC applications. Paste and powder are the two most common forms stocked locally.
What Brazing Flux Does During the Heating Process
Flux performs four jobs simultaneously once heat is applied. Understanding each one helps you select the right product for your base metal and temperature range.
Shields from Air
Forms a physical barrier over the heated metal, blocking oxygen from reaching the surface and stopping fresh oxide from building up.
Cleans the Metal
Chemically dissolves and absorbs existing oxides so the filler metal contacts bare, reactive metal rather than a contaminated surface.
Improves Filler Flow
Reduces surface tension so the molten filler spreads and draws into tight joint gaps through capillary action rather than beading up at the surface.
Shows the Temperature
Changes appearance at known temperature thresholds. When it turns completely clear and glassy, the joint is ready to receive the filler rod.
The Four Visual Stages of Flux as It Heats
| Temperature |
Visual State |
What It Means |
| 212 F / 100 C |
Water evaporates off |
Do not heat too fast here. Rapid boiling pushes the flux off the joint before it can protect anything. |
| 600 F / 316 C |
White, puffy |
Even puffing across the joint confirms even heat distribution. Uneven puffing signals a hot spot. |
| 800 F / 427 C |
Cloudy, spreading |
Flux has spread into a protective blanket. The metal is being shielded from air. |
| 1100 F / 593 C |
Clear liquid |
Metal is fully clean and at working temperature. Apply the filler rod now. |
Which Brazing Flux Types Are Available in Saudi Arabia?
Saudi distributors stock four main flux categories. The metal you are joining determines which one you need. Using the wrong flux for the base metal means the flux will either burn off before the filler flows, fail to dissolve the oxide layer, or leave corrosive residue that weakens the joint over time.
White Brazing Flux for Silver Alloy and Copper Pipe Work
White flux is the most commonly requested product across Saudi distributors. It is formulated for silver brazing alloys and works reliably on copper, brass, and stainless steel. The paste form is applied to the joint and rod before heating. It turns completely liquid at brazing temperature, leaving a clean metal surface ready for the filler.
Typical Use Cases
Refrigeration copper lines, HVAC copper pipe joints, brass fittings, stainless steel food equipment joints, and general silver brazing with 30 to 56 percent silver alloy rods.
Borax-Based Brazing Flux for Steel and Brass Applications
Borax flux is the standard choice for bronze rod brazing on mild steel, carbon steel, and brass. It is available in powder form and works at higher temperatures than white flux, typically above 800 degrees Celsius. Borax is the most economical flux option and is widely stocked at welding supply shops across Riyadh, Dammam, and Jeddah.
Typical Use Cases
Steel pipe brazing, bronze welding rod applications, brass-to-steel joints, maintenance workshop repairs, and general fabrication where bronze or brass filler is used.
Aluminium Brazing Flux for HVAC, Refrigeration, and Automotive Repair
Aluminium oxidizes almost instantly when heated, forming a layer that standard flux cannot penetrate. Aluminium-specific flux contains chloride and fluoride compounds that chemically break through this barrier. This flux is significantly more aggressive than other types and requires thorough post-braze cleaning to prevent corrosion from residue. Flux-47 and similar chloride-fluoride formulations are available in 0.5 kg containers from several Saudi suppliers.
Typical Use Cases
Air conditioner aluminium coil repair, automotive radiator work, aluminium heat exchanger maintenance, and refrigeration component joining where aluminium to aluminium or aluminium to copper transitions are required.
High Temperature Brazing Flux for Industrial Furnace and Heavy Fabrication Work
Standard flux burns off above 900 to 950 degrees Celsius. If your brazing process requires temperatures between 950 and 1200 degrees Celsius, you need a high-temperature formulation. These are used in heavy industrial fabrication, tool steel work, and furnace brazing applications. Products like BOHLER BW XII and specialty high-temp pastes from ESAB cover this range. Stock availability in Saudi Arabia is more limited for this category and usually requires ordering through an industrial distributor rather than a local welding shop.
Brazing Flux Forms: Paste, Powder, and Flux-Coated Rods
Paste and Liquid Flux for Precise Joint Application
Paste is the most commonly used form across Saudi workshops. It is brushed or spatula-applied directly onto both the joint surfaces and the filler rod tip before heating. Paste clings to vertical surfaces and is less likely to fall off than powder during positioning. Harris Stay-Silv white brazing flux paste is one of the most frequently requested products from Saudi welding distributors. Available in containers ranging from small 60 g workshop tubs to 1 kg industrial tins.
Powder Flux for High Volume and Furnace Brazing Applications
Powder flux is used by dipping the heated end of the brazing rod directly into the container. The rod picks up flux as it enters the joint. This is faster for high-volume work and works well in automated or semi-automated setups. Powder is also used in furnace brazing where paste would lose its consistency during pre-heating. Arcos Brass Brazing Flux Powder in 100 g containers is a common item stocked by Saudi industrial suppliers. Larger bags of 500 g and 1 kg are available through distributors in Dammam and Jubail for production environments.
Flux-Coated Brazing Rods to Eliminate Manual Application
Flux-coated rods carry a pre-applied flux layer directly on the rod. No separate flux container is needed at the workstation. The brazing rod Safety Silv 45 with flux coating is an example of this format and is available through Harris distributors in Saudi Arabia. These rods are useful for field technicians and maintenance crews who cannot carry multiple products to a job site. The flux layer activates as the rod approaches the heated joint, performing the same function as separately applied paste.
Brazing Flux Brands and Specific Products Stocked in Saudi Arabia
Harris Stay-Silv Brazing Flux - White Paste and Powder
Harris Products Group
Harris Stay-Silv white brazing flux is a borate-based paste used with silver brazing alloys on copper, brass, bronze, and stainless steel. The SSWF1 model is the most recognized. Operating range is 565 to 870 degrees Celsius. Compatible with Harris Safety-Silv 45 and Safety-Silv 56 alloy rods.
| Product Code |
SSWF1 (1 lb paste), SSB1 (powder) |
| Working Temperature |
565 to 870 C (1050 to 1600 F) |
| Metals Covered |
Copper, brass, bronze, stainless steel |
| Form |
Paste and powder |
Arcos Brass Brazing Flux Powder for Workshop and Maintenance Use
Arcos
Available in 100 g containers. Used for brass rod brazing on steel and iron. Powder format is well suited to maintenance teams and job-site applications. Dip the heated rod tip into the powder before applying to the joint. Compatible with standard bronze and brass brazing rods.
| Pack Size |
100 g container |
| Application Method |
Rod dip application |
| Suitable Filler |
Bronze rod, brass brazing alloy |
Flux-47 Aluminium Brazing Flux for Refrigeration Technicians
Industrial Formulation
Flux-47 is a chloride and fluoride based flux designed specifically for aluminium brazing. It is sold in 0.5 kg containers and is used extensively by HVAC and refrigeration technicians in Saudi Arabia for aluminium coil repair and joining. Post-braze, all residue must be washed off with hot water to prevent long-term corrosion from the aggressive chloride chemistry.
Important
Aluminium flux residue is corrosive. Always clean the joint with hot water immediately after brazing. Do not leave residue on the metal.
BOHLER BW XII and ESAB Brazing Fluxes for Industrial Fabrication
BOHLER BW XII and ESAB branded brazing fluxes are specified for heavy industrial fabrication, construction, and high-temperature applications. These products are distributed through industrial welding supply companies in the Eastern Province and Riyadh. They are typically sold in larger quantities, starting at 1 kg, and are available through Alruqee Industrial Marketing and Abahsain Welding Division for projects requiring certified materials and technical datasheets.
HOT Max Brazing Flux Powder for Budget-Conscious Applications
HOT Max is a lower-cost powder flux option used in small workshops and by independent maintenance technicians. Available in standard container sizes through online procurement and some welding supply shops. Best suited for general-purpose steel and brass work where certified flux is not required by the project specification.
Which Brazing Flux Should You Use for Your Specific Metals?
| Base Metal |
Recommended Flux |
Filler Type |
Form to Use |
| Copper to Copper |
White brazing flux |
Silver 45 or 56% |
Paste |
| Copper to Brass |
White brazing flux |
Silver 30-45% |
Paste |
| Steel to Steel |
Borax-based flux |
Bronze rod |
Powder or paste |
| Stainless Steel |
White brazing flux |
Silver 50-56% |
Paste |
| Aluminium to Aluminium |
Aluminium flux (Flux-47) |
Aluminium alloy rod |
Powder |
| Steel to Copper |
White brazing flux |
Silver 45% |
Paste |
Brazing Flux Suppliers and Distributors in Saudi Arabia
These are verified industrial distributors supplying brazing flux across Riyadh, Jeddah, the Eastern Province, Dammam, and Jubail. Most carry stock for same-day or next-day pickup. For bulk orders and site delivery, contact the distributor directly to confirm lead time and minimum quantities.
Cool Plus Trading EST.
Riyadh, Saudi Arabia
Riyadh
Cool Plus Trading is a welding and industrial supply distributor operating in Riyadh. They supply brazing flux products including silver brazing flux and copper brazing flux to workshops, HVAC contractors, and maintenance companies. They serve both retail buyers and B2B accounts with credit terms available for registered companies.
Address
Asad Ibn Al Fourat, Al Amal, Riyadh, KSA
Contact
+966 11 401 2051
Mobile: +966 54 343 2650
| Products Stocked |
Silver brazing flux, copper brazing flux, brazing rods and flux paste |
| Delivery Coverage |
Riyadh local delivery available. Shipping to other regions on request. |
| Lead Time |
Same-day or next-day for stock items in Riyadh |
| Sectors Served |
HVAC, refrigeration, general fabrication, maintenance workshops |
Alruqee Industrial Marketing Company
Al Khobar, Eastern Province
Eastern Province
Alruqee is one of the larger industrial marketing companies in the Eastern Province, supplying welding consumables, brazing materials, and industrial gases to oil and gas contractors, construction companies, and fabrication facilities. They carry ESAB, BOHLER, and other certified brands and are able to provide material test certificates and product datasheets for project-spec procurement.
Address
Alkhobar 31952, Kingdom of Saudi Arabia
| Products Stocked |
ESAB brazing flux, BOHLER BW XII, silver brazing flux paste, high temp flux, flux powder |
| Certifications |
Material test certificates available. ISO-compliant supply chain for oil and gas projects. |
| Delivery Coverage |
Eastern Province, Jubail, Dammam, Dhahran. Nationwide shipping available for bulk orders. |
| Minimum Order |
No stated minimum for standard items. Bulk pricing available from 10 kg and above. |
| Sectors Served |
Oil and gas, petrochemical, heavy fabrication, construction, maintenance contractors |
Saleh and Abdulaziz Abahsain Co. - Welding Division
Dammam and Eastern Province | Lincoln Electric Distributor
Dammam
The Abahsain Welding Division is the authorized Lincoln Electric distributor for Saudi Arabia and one of the most established welding consumables companies in the Eastern Province. They handle brazing consumables including flux and filler alloys for industrial clients across the oil, gas, petrochemical, and construction sectors. Project-level technical support and welding procedure qualification assistance is available.
| Coverage Area |
Dammam, Al Khobar, Jubail, Eastern Province, with national shipping |
| Brand Portfolio |
Lincoln Electric brazing products, Harris, and other major welding consumable brands |
| Technical Support |
Welding engineers available for product selection and procedure qualification |
| Certifications |
Products available with mill certificates, MSDS, and COC documentation for project compliance |
Additional Brazing Flux Distributors in Dammam and Eastern Province
Welding and Cutting Products - Industrial Supplies Development Co.
Dammam, Eastern Province
Industrial welding consumables and brazing supplies. Stocks cutting and welding accessories for fabrication facilities and maintenance contractors across the Eastern Province.
United Suppliers Est. for Industrial Services
Dammam, Eastern Province
Industrial equipment and welding-related consumables. Serves maintenance teams and fabrication workshops with welding, brazing, and cutting products.
RUWWAD Industrial Trading EST.
Jubail Industrial City
Industrial gases and welding materials supplier serving the Jubail industrial zone. Stocks brazing consumables for petrochemical and process plant maintenance.
Saudi Welding Co. for Trading and Marketing
Jubail and Jeddah
Multi-branch welding consumables company with locations in Jubail and Jeddah. Stocks brazing flux, brazing rods, and related accessories for general industrial use.
Brazing Flux Suppliers in Riyadh
| Company |
Location |
Specialization |
| Spark Weld Trading Company |
Riyadh |
Welding consumables and brazing supplies for fabrication workshops |
| DAC Saudi Arabia |
Riyadh and branches |
Welding materials portfolio explicitly includes brazing rods and fluxes. Online ordering available at dacksa.com |
| Saudi Welding Company (Riyadh branch) |
Riyadh |
General welding consumables for light and medium industry |
Brazing Flux Suppliers in Jeddah
Saudi Welding Co. for Trading and Marketing
Jeddah
Welding and brazing consumables serving the Jeddah industrial zone and surrounding workshops.
Hasan Mohamed AlMahroos
Jeddah
Industrial equipment and supply company with welding consumable products including brazing materials for general industrial applications.
How to Remove Brazing Flux Residue After Joining
Removing White Flux and Borax Residue from Copper and Steel
Once the joint has cooled slightly but is still warm, submerge or flush it with hot water. Most white flux and borax residue is water-soluble and washes off cleanly at this stage. If residue has hardened after full cooling, soak the joint in hot water for several minutes and scrub with a wire brush. Do not use acid cleaners on copper plumbing unless you are certain the product is compatible with the solder or filler you used.
Removing Aluminium Flux Residue - Why It Cannot Be Left in Place
Aluminium flux contains aggressive chloride and fluoride salts that continue reacting with the base metal after the braze is complete. If left in place, flux residue on aluminium joints causes accelerated corrosion that can fail the joint within weeks in humid conditions. Flush with hot water immediately after the joint cools to handling temperature. For enclosed joints or tubes, flush water through the interior. In refrigeration work, confirm all residue is removed before pressurizing the system, as residue contamination in refrigerant lines creates additional service problems.
Brazing Flux Pricing in Saudi Arabia
Brazing flux pricing varies by type, brand, and quantity. General price ranges for the Saudi market as of 2025 are as follows. For exact current pricing, contact the supplier directly or request a quotation for bulk orders.
| Product |
Size |
Approximate Price Range (SAR) |
| Borax flux powder (general) |
100 g |
15 to 35 SAR |
| White brazing flux paste (Harris or equivalent) |
500 g / 1 lb |
45 to 120 SAR |
| Aluminium flux (Flux-47) |
500 g |
60 to 150 SAR |
| Silver brazing flux paste (brand name) |
1 kg |
200 to 450 SAR |
| High temp flux (BOHLER BW XII or ESAB) |
1 kg |
Contact supplier for quotation |
Procurement Note
For bulk procurement above 10 kg, request a formal quotation from Alruqee, Abahsain Welding Division, or DAC Saudi Arabia. These distributors offer volume pricing and can arrange delivery to project sites in Riyadh, Jeddah, Dammam, Jubail, and Yanbu. Always confirm the product datasheet and temperature range match your application before placing a large order.
People Also Ask: Brazing Flux
What is brazing flux used for?
Prevents oxidation when metal is heated with a torch.
Dissolves existing oxides so filler metal can bond to bare metal.
Lowers surface tension so molten filler flows into the joint gap.
Changes color as it heats, showing you when the metal is ready for the filler rod.
Is brazing flux the same as soldering flux?
No. Different chemistry, different temperature range.
Soldering Flux
Below 450 C. Rosin or mild acid base. Burns off fast.
Brazing Flux
450 to 1200 C. Borate or fluoride base. Stays active at heat.
Can I braze without flux?
For torch brazing in open air: No.
Without flux, the metal oxidizes as it heats and the filler cannot bond.
Exception: furnace brazing in a controlled nitrogen or hydrogen atmosphere replaces flux entirely. Not practical for workshop or field work.
What flux is most commonly used in brazing?
Steel and brass with bronze rod: Borax powder
Copper, brass, stainless with silver alloy: White brazing flux paste (Harris Stay-Silv)
Aluminium: Chloride-fluoride flux (Flux-47). Standard borax will not work on aluminium.
What does flux do in brazing?
1. Shields the metal from air while it heats
2. Dissolves and absorbs existing oxide from the surface
3. Reduces surface tension so molten filler flows deeper into the joint
4. Turns clear at working temperature, signaling when to apply the rod
What makes brazing filler metal flow into the joint?
Capillary action pulls molten filler into tight gaps between the base metals.
Flux lowers surface tension so the filler travels further into the gap.
Correct joint clearance: 0.05 to 0.2 mm for most silver alloys.
Note: filler always flows toward heat. If one side is hotter, the filler goes there, not into the gap evenly.
What is brazing flux in welding?
Brazing and welding are different processes. In welding, the base metal melts. In brazing, only the filler melts.
Brazing flux is the compound that keeps the metal clean and oxide-free during the braze.
In workshops, the term is often used loosely to include bronze rod applications, which also operate in the brazing temperature range.
What is brazing flux made of?
White flux (silver brazing): Borate and fluoride compounds in a water-based paste
Borax flux (steel, brass): Sodium borate, sometimes with boric acid
Aluminium flux: Potassium chloride and potassium fluoride
High temp flux: Extended borate-fluoride blend to stay active above 950 C
What are brazing flux powder names available in Saudi Arabia?
Harris Stay-Silv Brazing Flux Powder
Arcos Brass Brazing Flux Powder (100 g)
HOT Max Brazing Flux Powder
S Pro Flux Low Temperature Brazing Powder
Flux-47 Aluminium Brazing Flux Powder (0.5 kg)
How do you use brazing flux powder?
1. Warm the rod tip with the torch to around 200 to 300 C
2. Dip the rod tip into the powder. It sticks to the warm rod.
3. Heat the base metal, not the rod
4. When the flux on the rod turns clear, touch the rod to the joint
Alternative: mix powder with water to make a paste, brush onto the joint before heating.
What is brazing flux liquid and when do you use it?
A thin, water-based version of paste flux. Same chemistry, easier to apply in tight spots.
Good for pre-assembled joints where a brush cannot reach.
Used in automated brazing equipment with flux-injection systems.
Dries faster than paste. Apply just before heating, not during prep.
What is copper brazing flux?
Any brazing flux rated for copper base metal. White paste flux is the standard choice.
Apply to both the pipe and fitting before heating.
Use with silver 45 or 56 percent alloy rod for copper-to-copper or copper-to-brass joints.
Stocked by: Harris, Castolin, ESAB. Available through Alruqee, Cool Plus Trading, and Abahsain Welding Division.
What are the three types of brazing flux?
1. Borax-based for steel and brass at higher temperatures
2. White borate-fluoride flux for silver brazing on copper, brass, stainless
3. Aluminium chloride-fluoride flux for aluminium only. The other two will not work on aluminium.
Can I use Vaseline as flux?
No. Not for brazing.
Vaseline is petroleum jelly. It burns off within seconds at brazing temperatures.
It does no chemical oxide removal and leaves carbon residue that contaminates the joint.
It is sometimes used in soft soldering below 200 C only. For brazing, use a flux rated for your temperature range.
Not Sure Which Flux to Order?
Tell any supplier on this page two things:
1. The metals you are joining, for example copper to steel, aluminium to aluminium
2. The filler rod you are using, for example silver solder 45 percent, bronze rod, or aluminium alloy